The alloy AlFeSi is alloyed for increasing the strength increase with Fe and Si. The material belongs to the nature-hard aluminum materials. A strength increase can be achieved only by cold forming. The alloy AlFeSi is very well cold and warm formable and has a good thermal and relatively good electrical conductivity. The material is particularly suitable for deep-drawing. It is well solderable. The material is to be oxidized well anodically, i.e. a shining clean surface develops. It is standardised as sheet metal or strip (DIN 1788 and DIN 1745). Application: for screw-type caps, for menu bowls, for light containers, bottle caps, cover containers and other form packing, for metal goods, like trim, decorated tiles, flexible pipes, various deep-drawing products, for heat exchangers and radiator fins

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

O

EN 573-3, EN 1396, EN 485, EN 546, EN 683

20.0 °C

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

O

EN 573-3, EN 1396, EN 485, EN 546, EN 683

Elongation

1.0 %

Show Material materials with Elongation of 1.0 %

O

EN 573-3, EN 546

A50

3.0 %

Show Material materials with Elongation of 3.0 %

O

EN 573-3, EN 546

A50

4.0 %

Show Material materials with Elongation of 4.0 %

O

EN 573-3, EN 546

A50

7.0 %

Show Material materials with Elongation of 7.0 %

O

EN 573-3, EN 546

A50

12.0 %

Show Material materials with Elongation of 12.0 %

O

EN 573-3, EN 546, EN 683

A50

16.0 %

Show Material materials with Elongation of 16.0 %

O

EN 573-3, EN 546, EN 683

A50

19.0 %

Show Material materials with Elongation of 19.0 %

O

EN 573-3, EN 1396, EN 485

A50

20.0 %

Show Material materials with Elongation of 20.0 %

O

EN 573-3, EN 683

A50

21.0 %

Show Material materials with Elongation of 21.0 %

O

EN 573-3, EN 1396, EN 485

A50

24.0 %

Show Material materials with Elongation of 24.0 %

O

EN 573-3, EN 1396, EN 485

A50

25.0 %

Show Material materials with Elongation of 25.0 %

O

EN 573-3, EN 485

A50

30.0 %

Show Material materials with Elongation of 30.0 %

O

EN 573-3, EN 485

A50

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

A100

20.0 °C

10.0 %

Show Material materials with Elongation of 10.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

A100

20.0 °C

15.0 %

Show Material materials with Elongation of 15.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

A100

20.0 °C

20.0 %

Show Material materials with Elongation of 20.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

A100

20.0 °C

30.0 %

Show Material materials with Elongation of 30.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

A10

20.0 °C

35.0 %

Show Material materials with Elongation of 35.0 %

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

Hardness, Brinell

25.0 [-]

Show Material materials with Hardness, Brinell of 25.0 [-]

O

EN 573-3, EN 485

20.0 °C

25.0 [-]

Show Material materials with Hardness, Brinell of 25.0 [-]

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 8000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 8000 Series Aluminium

Tensile strength

50.0 - 110.0 MPa

Show Material materials with Tensile strength of 50.0 - 110.0 MPa

O

EN 573-3, EN 546

55.0 - 115.0 MPa

Show Material materials with Tensile strength of 55.0 - 115.0 MPa

O

EN 573-3, EN 546

55.0 - 120.0 MPa

Show Material materials with Tensile strength of 55.0 - 120.0 MPa

O

EN 573-3, EN 546

65.0 - 130.0 MPa

Show Material materials with Tensile strength of 65.0 - 130.0 MPa

O

EN 573-3, EN 546, EN 683

80.0 - 120.0 MPa

Show Material materials with Tensile strength of 80.0 - 120.0 MPa

O

EN 573-3, EN 1396

85.0 MPa

Show Material materials with Tensile strength of 85.0 MPa

O

EN 573-3, EN 485

20.0 °C

75.0 - 110.0 MPa

Show Material materials with Tensile strength of 75.0 - 110.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

20.0 °C

75.0 - 115.0 MPa

Show Material materials with Tensile strength of 75.0 - 115.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

20.0 °C

80.0 - 110.0 MPa

Show Material materials with Tensile strength of 80.0 - 110.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

20.0 °C

80.0 - 115.0 MPa

Show Material materials with Tensile strength of 80.0 - 115.0 MPa

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

O

EN 573-3, EN 1396, EN 485, EN 546, EN 683

100 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

O

EN 573-3, EN 1396, EN 485, EN 546, EN 683

Melting point

640.0 - 655.0 °C

Show Material materials with Melting point of 640.0 - 655.0 °C

O

EN 573-3, EN 1396, EN 485, EN 546, EN 683

Specific heat capacity

920.0 J/(kg·K)

Show Material materials with Specific heat capacity of 920.0 J/(kg·K)

Typical for Wrought 8000 Series Aluminium

Thermal conductivity

20.0 °C

210.0 - 220.0 W/(m·K)

Show Material materials with Thermal conductivity of 210.0 - 220.0 W/(m·K)

O

DIN 1725-1, EN 573-3, EN 573-4, EN 1396, EN 485, EN 546, EN 683

Flat

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

34000000.0 - 35000000.0 S/m

Show Material materials with Electrical conductivity of 34000000.0 - 35000000.0 S/m

O

DIN 1725-1, EN 573-3, EN 573-4, EN 1396, EN 485, EN 546, EN 683

Flat

Electrical resistivity

2.86e-08 - 2.94e-08 Ω·m

Show Material materials with Electrical resistivity of 2.86e-08 - 2.94e-08 Ω·m

O

EN 573-3, EN 1396, EN 485, EN 546, EN 683

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

O

EN 573-3, EN 1396, EN 485, EN 546, EN 683

Copper

0.1 %

Show Material materials with Copper of 0.1 %

O

DIN 1725-1, EN 573-3, EN 573-4, EN 1396, EN 485, EN 546, EN 683

Flat

Iron

0.5 - 1.0 %

Show Material materials with Iron of 0.5 - 1.0 %

O

DIN 1725-1, EN 573-3, EN 573-4, EN 1396, EN 485, EN 546, EN 683

Flat

Magnesium

0.1 %

Show Material materials with Magnesium of 0.1 %

O

EN 573-3, EN 1396, EN 485, EN 546, EN 683

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

O

DIN 1725-1, EN 573-3, EN 573-4, EN 1396, EN 485, EN 546, EN 683

Flat

Silicon

0.4 - 0.8 %

Show Material materials with Silicon of 0.4 - 0.8 %

O

DIN 1725-1, EN 573-3, EN 573-4, EN 1396, EN 485, EN 546, EN 683

Flat

Titanium

0.05

Show Material materials with Titanium of 0.05

O

DIN 1725-1, EN 573-3, EN 573-4

Flat

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

O

DIN 1725-1, EN 573-3, EN 573-4, EN 1396, EN 485, EN 546, EN 683

Flat