Biegemodul: 17.5 GPa

Quick Comparison

Polyethylenterephthalat (PET)

Arnite® AV2 390

Geliefert von:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® Ace MX53B

Geliefert von:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® NMX33

Geliefert von:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® Ace WX53-FC

Geliefert von:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® XS81B

Geliefert von:

DSM Engineering Materials

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DC0041PR

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00CSXP

Geliefert von:

Sabic