Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Kohlenstoffarmer Stahl
EN 10132-4 Grade C125S quenched and tempered (+QT)Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 THMedium Carbon Steel
DIN 17222 Grade C55 cold rolled and hardenedMedium Carbon Steel
DIN 17222 Grade Ck55 cold rolled and hardenedMedium Carbon Steel
EN 10132-3 Grade C50E quenched and tempered (+QT)Medium Carbon Steel
EN 10132-3 Grade C55E quenched and tempered (+QT)Silicon Steel
DIN 17222 Grade 55Si7 cold rolled and hardenedMedium Carbon Steel
EN 10132-4 Grade C55S quenched and tempered (+QT)