General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.86 g/cm³ Show Material materials with Density of 7.86 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for High Carbon Steel |
Hardness, Rockwell C | 23.0 °C | 38.5 - 54 [-] Show Material materials with Hardness, Rockwell C of 38.5 - 54 [-] | |
Hardness, Vickers | 23.0 °C | 370 - 580 [-] Show Material materials with Hardness, Vickers of 370 - 580 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for High Carbon Steel |
Shear modulus | 23.0 °C | 81 GPa Show Material materials with Shear modulus of 81 GPa | Typical for High Carbon Steel |
Tensile strength | 23.0 °C | 1200 - 1900 MPa Show Material materials with Tensile strength of 1200 - 1900 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.32E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K | Typical for High Carbon Steel |
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1400 - 1500 °C Show Material materials with Melting point of 1400 - 1500 °C | ||
Specific heat capacity | 23.0 °C | 486 J/(kg·K) Show Material materials with Specific heat capacity of 486 J/(kg·K) | Typical for High Carbon Steel |
Thermal conductivity | 23.0 °C | 36 W/(m·K) Show Material materials with Thermal conductivity of 36 W/(m·K) | Typical for High Carbon Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.7 - 0.8 % Show Material materials with Carbon of 0.7 - 0.8 % |
Chromium | 0 - 0.4 % Show Material materials with Chromium of 0 - 0.4 % |
Iron | Balance |
Manganese | 0.6 - 0.9 % Show Material materials with Manganese of 0.6 - 0.9 % |
Molybdenum | 0 - 0.1 % Show Material materials with Molybdenum of 0 - 0.1 % |
Nickel | 0 - 0.4 % Show Material materials with Nickel of 0 - 0.4 % |
Phosphorus | 0 - 0.25 % Show Material materials with Phosphorus of 0 - 0.25 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 0 - 0.25 % Show Material materials with Sulfur of 0 - 0.25 % |
Technological properties
Property | ||
---|---|---|
Processing history | Quenched and tempered |