Tungsten Bright Foil

Want to keep this datasheet? Save it now in your required format

Description

Tungsten has the highest melting point of all metals and is therefore also suitable for very high-temperature applications. It is also characterized by a uniquely low coefficient of thermal expansion and a very high level of dimensional stability.

Related Standards

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

19.2 g/cm³

Show Supplier Material materials with Density of 19.2 g/cm³

Neutron capture cross-section

23.0 °C

0 m²

Show Supplier Material materials with Neutron capture cross-section of 0 m²

Dimension

PropertyValue

Length

600 mm

Show Supplier Material materials with Length of 600 mm

Thickness

0.05 mm

Show Supplier Material materials with Thickness of 0.05 mm

Width

160 mm

Show Supplier Material materials with Width of 160 mm

Mechanical

PropertyTemperatureValue

Hardness, Vickers

23.0 °C

550 [-]

Show Supplier Material materials with Hardness, Vickers of 550 [-]

Thermal

PropertyValue

Melting point

3420 °C

Show Supplier Material materials with Melting point of 3420 °C

Electrical

PropertyTemperatureValue

Electron work function

23.0 °C

4.54 eV

Show Supplier Material materials with Electron work function of 4.54 eV

Acoustical

PropertyTemperatureValue

Sound speed, longitudinal

23.0 °C

5180 m/s

Show Supplier Material materials with Sound speed, longitudinal of 5180 m/s

Sound speed, transversal

23.0 °C

2870 m/s

Show Supplier Material materials with Sound speed, transversal of 2870 m/s

Chemical properties

PropertyValue

Aluminium

1E-4 %

Show Supplier Material materials with Aluminium of 1E-4 %

Cadmium

1E-4 %

Show Supplier Material materials with Cadmium of 1E-4 %

Carbon

6E-4 %

Show Supplier Material materials with Carbon of 6E-4 %

Chromium

3E-4 %

Show Supplier Material materials with Chromium of 3E-4 %

Copper

1E-4 %

Show Supplier Material materials with Copper of 1E-4 %

Iron

8E-4 %

Show Supplier Material materials with Iron of 8E-4 %

Lead

1E-4 %

Show Supplier Material materials with Lead of 1E-4 %

Molybdenum

1.2E-3 %

Show Supplier Material materials with Molybdenum of 1.2E-3 %

Nickel

2E-4 %

Show Supplier Material materials with Nickel of 2E-4 %

Oxygen

2E-4 %

Show Supplier Material materials with Oxygen of 2E-4 %

Potassium

1E-4 %

Show Supplier Material materials with Potassium of 1E-4 %

Silicon

1E-4 %

Show Supplier Material materials with Silicon of 1E-4 %

Tungsten

99.97 %

Show Supplier Material materials with Tungsten of 99.97 %

Technological properties

Property
Application areas

Premium Quality sheets are used for many applications where superior finish is desired. It is ideal for deep drawing.