White Cast Iron
EN 12513 Grade G-X 300 CrNiSi 9 5 2White Cast Iron
EN 12513 Grade G-X 330 NiCr 4 2White Cast Iron
EN 12513 Grade G-X 260 NiCr 4 2Aluminosilikat
General Aluminosilicate GlassGusseisen
ASTM A532 Class I Type BGusseisen
ASTM A532 Class I Type CAluminosilikat
General Aluminosilicate Display GlassGusseisen
ASTM A532 Class I Type A