ASTM A532 Class I Type A

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyValueTemperature

Hardness, Brinell

600 [-]

Show Material materials with Hardness, Brinell of 600 [-] at 23.0 °C

23.0 °C

Hardness, Rockwell C

56 [-]

Show Material materials with Hardness, Rockwell C of 56 [-] at 23.0 °C

23.0 °C

Hardness, Vickers

660 [-]

Show Material materials with Hardness, Vickers of 660 [-] at 23.0 °C

23.0 °C

Chemical properties

Property

Carbon

2.8 - 3.6 %

Chromium

1.4 - 4 %

Manganese

2 %

Molybdenum

1 %

Nickel

3.3 - 5 %

Phosphorus

0.3 %

Silicon

0.8 %

Sulfur

0.15 %