General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.7 g/cm³ Show Material materials with Density of 7.7 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 169 - 183 GPa Show Material materials with Elastic modulus of 169 - 183 GPa | |
Hardness, Brinell | 20.0 °C | 430 - 690 [-] Show Material materials with Hardness, Brinell of 430 - 690 [-] | |
Hardness, Vickers | 20.0 °C | 450 - 750 [-] Show Material materials with Hardness, Vickers of 450 - 750 [-] | |
Poisson's ratio | 23.0 °C | 0.27 [-] Show Material materials with Poisson's ratio of 0.27 [-] | Typical for Cast Iron |
Shear modulus | 23.0 °C | 41 GPa Show Material materials with Shear modulus of 41 GPa | Typical for Cast Iron |
Tensile strength | 20.0 °C | 280 - 350 MPa Show Material materials with Tensile strength of 280 - 350 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 1/K | Typical for White Cast Iron |
Melting point | 1209 °C Show Material materials with Melting point of 1209 °C | Typical for White Cast Iron | |
Specific heat capacity | 23.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | Typical for White Cast Iron |
Thermal conductivity | 20.0 °C | 14 W/(m·K) Show Material materials with Thermal conductivity of 14 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 8E-7 Ω·m Show Material materials with Electrical resistivity of 8E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbon | 3 - 3.6 % Show Material materials with Carbon of 3 - 3.6 % |
Chromium | 1.4 - 2.4 % Show Material materials with Chromium of 1.4 - 2.4 % |
Manganese | 0.3 - 0.7 % Show Material materials with Manganese of 0.3 - 0.7 % |
Molybdenum | 0.5 % Show Material materials with Molybdenum of 0.5 % |
Nickel | 3.3 - 5 % Show Material materials with Nickel of 3.3 - 5 % |
Silicon | 0.2 - 0.8 % Show Material materials with Silicon of 0.2 - 0.8 % |
Do you have a technical question or need more information about this material?