Heat deflection temperature, 0.45 MPa: 51 °C

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2750-01

Geliefert von:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2950-05

Geliefert von:

Arkema: High Performance Polymers

Thermoplast

extrudr Pearl Filament

Geliefert von:

Extrudr