Heat deflection temperature, 1.80 MPa: 223 °C

Quick Comparison

Polyimid (PI)

EXTEM™ Resin XH1015 - Europe

Geliefert von:

Sabic

Polyimid (PI)

EXTEM™ Resin XH1015 - Asia

Geliefert von:

Sabic

Polyimid (PI)

EXTEM™ Resin XH1015 - Americas

Geliefert von:

Sabic

Polyethersulfon (PES)

LNP™ LUBRICOMP™ Compound JCL36

Geliefert von:

Sabic

Polyethylenterephthalat (PET)

VYPET™ VNT-630

Geliefert von:

Lavergne