Impact strength, Charpy notched, ASTM: 65 J/m

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 705

Geliefert von:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 370

Geliefert von:

Arkema: High Performance Polymers

Polypropylen (PP)

PP GF30

Geliefert von:

Xiamen Keyuan Plastic Co., Ltd

Polyoxymethylen (POM)

POM GB25

Geliefert von:

Xiamen Keyuan Plastic Co., Ltd