POM GB25

Alternative and trade names
POM-GB25
Want to keep this datasheet? Save it now in your required format

Description

Polyoxymethylene (POM) reinforced with 20% glass beads

This material data has been provided by Xiamen Keyuan Plastic Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.6 g/cm³

Show Supplier Material materials with Density of 1.6 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

3.2 GPa

Show Supplier Material materials with Flexural modulus of 3.2 GPa

ASTM D790

Flexural strength

23.0 °C

83 MPa

Show Supplier Material materials with Flexural strength of 83 MPa

ASTM D790

Impact strength, Charpy notched, ASTM

23.0 °C

65 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 65 J/m

ASTM D256

Tensile strength

23.0 °C

44 MPa

Show Supplier Material materials with Tensile strength of 44 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature

120 °C

Show Supplier Material materials with Heat deflection temperature of 120 °C

ASTM D648

Melting point

166 °C

Show Supplier Material materials with Melting point of 166 °C

ASTM D2117

Flammability

UL 94 HB (1.6mm)

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

3.7 [-]

Show Supplier Material materials with Dielectric constant of 3.7 [-]

ASTM D147

Dielectric strength

23.0 °C

19 kV/mm

Show Supplier Material materials with Dielectric strength of 19 kV/mm

ASTM D147

Technological properties

Property
Fillers

20% Glass Bead