Impact strength, Izod unnotched, ASTM: 907 J/m

Quick Comparison

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DF003E

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFL36XXY

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DX06409

Geliefert von:

Sabic

Polyamide 6 (PA6)

LNP™ STAT-KON™ Compound PFD06

Geliefert von:

Sabic

Duroplast-Polymer-matrix-verbundwerkstoff

Silicone MC507U - Sheet

Geliefert von:

Norplex-Micarta

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QFP36

Geliefert von:

Sabic

Polyamide 12 (PA12)

LNP™ LUBRICOMP™ Compound SFL2A

Geliefert von:

Sabic