Silicone MC507U - Sheet

Alternative and trade names
NEMA GRADE: G-7, Type, U.L. LISTED: N
Want to keep this datasheet? Save it now in your required format

Description

MC507U is a utility grade, glass fabric combined with a silicone resin system. MC507U has excellent strength and electrical properties. MC507U complies with MIL-I-24768/17 – GSG, with the exception of some specific electrical properties.

This material data has been provided by Norplex Micarta.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bonding strength

23.0 °C

340.2 Kg

Show Supplier Material materials with Bonding strength of 340.2 Kg

ASTM D229, Condition A

Density

23.0 °C

1.88 g/cm³

Show Supplier Material materials with Density of 1.88 g/cm³

ASTM D792

Moisture absorption

23.0 °C

0.19 %

Show Supplier Material materials with Moisture absorption of 0.19 %

ASTM D570, Condition D₁-24/23

Mechanical

PropertyTemperatureValueComment

Flexural strength

23.0 °C

167.5 MPa

Show Supplier Material materials with Flexural strength of 167.5 MPa

ASTM D790, Condition A

Flexural strength, transverse

23.0 °C

149.6 MPa

Show Supplier Material materials with Flexural strength, transverse of 149.6 MPa

ASTM D790, Condition A

Hardness, Rockwell M

23.0 °C

100 [-]

Show Supplier Material materials with Hardness, Rockwell M of 100 [-]

ASTM D785

Impact strength, Izod unnotched, ASTM

23.0 °C

907 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 907 J/m

ASTM D256, Condition E-48/50

Impact strength, Izod unnotched, ASTM, Transversal

23.0 °C

614 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM, Transversal of 614 J/m

ASTM D256, Condition E-48/50

Thermal

PropertyValueComment

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL Bulletin 746b¹

Relative temperature index, mechanical strength

220 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 220 °C

UL Bulletin 746b¹

Arc resistance

200 seconds, ASTM D495, Condition A

Flammability

UL Bulletin 94, Class V-0, Condition A

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

32 - 55 kV

Show Supplier Material materials with Breakdown voltage of 32 - 55 kV

ASTM D149, Condition D48/50 (Min.) & A (Max.)

Dielectric constant, 1MHz

23.0 °C

4.55 - 4.67 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 4.55 - 4.67 [-]

ASTM D150, Condition A (Min.) & D-24/23 (Max.)

Dielectric strength

23.0 °C

13.78 kV/mm

Show Supplier Material materials with Dielectric strength of 13.78 kV/mm

ASTM D149, Condition A

Dissipation factor, 1MHz

23.0 °C

0.02 - 0.05 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 - 0.05 [-]

Condition A (Min.) & D-24/23 (Max.)

Technological properties

Property
Application areas

It can be substituted for NEMA G-7, in most heating, appliance insulation and some bearing applications.

Fillers

Glass Fabric

Other

1.This temperature is a recommendation only, and based upon experience in various applications. The maximum operating temperature is dependent upon the application and should be investigated prior to use

Supplier Disclaimer

This data, while believed to be accurate and based on reliable analytical methods, is for informational purposes only. The terms and conditions of the agreement under which it is sold will govern any sales of this product. Data supplied above are "typical values"; not to be considered "specification values".


To assure the material's performance is adequate for a specific application; customers should verify, independent of Norplex-Micarta, performance characteristics of interest.


It is the responsibility of the users of this information to make sure that they have the latest version of this TDB, and are urged to check with Customer Service or, preferably our web site, www.norplex-micarta.com, to determine if the information is the most current available.