General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.64 g/cm³ Show Supplier Material materials with Density of 1.64 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.6 % Show Supplier Material materials with Moisture absorption of 0.6 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 16.1 GPa Show Supplier Material materials with Elastic modulus of 16.1 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 13.1 GPa Show Supplier Material materials with Flexural modulus of 13.1 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 241 MPa Show Supplier Material materials with Flexural strength of 241 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 112 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 112 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 112 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 112 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 907 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 907 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 149 MPa Show Supplier Material materials with Tensile strength of 149 MPa | ASTM D 638 | break |
Thermal
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |