Instrumented Impact, Total Energy: 37 J

Quick Comparison

Polypropylen (PP)

LNP™ STAT-KON™ Compound MX01767C

Geliefert von:

Sabic

Polyphenylether (PPE)

NORYL™ Resin PVX0901 - Asia

Geliefert von:

Sabic

Polymermischung (Blend)

NORYL PPX™ Resin PPX7115F - Americas

Geliefert von:

Sabic