General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 0.98 g/cm³ Show Supplier Material materials with Density of 0.98 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 0.98 [-] Show Supplier Material materials with Relative density of 0.98 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 1.6 GPa Show Supplier Material materials with Elastic modulus of 1.6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 18 % Show Supplier Material materials with Elongation of 18 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 1.5 GPa Show Supplier Material materials with Flexural modulus of 1.5 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 35 MPa Show Supplier Material materials with Flexural strength of 35 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 9 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 130 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 130 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 141 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 141 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1470 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1470 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 37 J Show Supplier Material materials with Instrumented Impact, Total Energy of 37 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 22 MPa Show Supplier Material materials with Tensile strength of 22 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9.2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9.2E-5 1/K | ASTM E 831 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 9.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9.5E-5 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature | 52 - 89 °C Show Supplier Material materials with Heat deflection temperature of 52 - 89 °C | ||
Heat deflection temperature, 0.45 MPa | 89 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 89 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 52 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 52 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Tray, Semiconductor, Electronic Material Handling, Industrial Material Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |