Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 soft annealed (+A)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT2)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT1)Austenitischer rostfreier Stahl
EN 10090 Grade X55CrMnNiN20-8 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
ASTM A213 Grade TP201 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A213 Grade TP202 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8S Class 1C, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8S Class 1D, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8SA Class 1C, Carbide solution treated in the finished conditionAustenitischer rostfreier Stahl
ASTM A240 Grade S20400 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade S21800 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade XM-17 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade XM-18 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 201-1 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 201-2 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A276 Grade S21800 Annealed; Hot-Finished or Cold-FinishedAustenitischer rostfreier Stahl
ASTM A249 Grade TP201 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A249 Grade TP202 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A479 Grade XM-17 AnnealedAustenitischer rostfreier Stahl
ASTM A479 Grade XM-18 Annealed