Schubmodule: 76 GPa

Quick Comparison

Medium Carbon Steel

EN 10028-3 Grade P355N normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Nickel Steel

EN 10028-4 Grade 11MnNi5-3 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 13MnNi6-3 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 15NiMn6 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

ASTM A353 Double-Normalized and Tempered

Geliefert von:

1 Matmatch-Lieferant

Seite 1 von 34