Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45E quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Steel
ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
DIN 17200 Grade C22 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17200 Grade C22 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10083-1 Grade C25E quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10083-1 Grade C25R quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10083-1 Grade C22 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10083-2 Grade C25 quenched and tempered (+QT)Medium Carbon Steel
ISO 683-1 Grade C45E normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
ISO 683-1 Grade C22E quenched and tempered (+QT)Kohlenstoffarmer Stahl
DIN 5512-1 Grade S355J2G3C normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10297-1 Grade 36Mn4 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10297-1 Grade Ck22 quenched and tempered (+QT)Medium Carbon Steel
ISO 683-1 Grade C45 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10277-2 Grade C10 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade C15 cold drawnKohlenstoffarmer Stahl
EN 10277-4 Grade C15R cold drawnMedium Carbon Steel
ISO 683-1 Grade C45 normalized or normalized formed (+N)Geliefert von: