Taber Abrasion: 76 mg/1000cy

Quick Comparison

Polyphenylether (PPE)

NORYL™ Resin N190X - Americas

Geliefert von:

Sabic

Polyphenylether (PPE)

NORYL™ Resin N190X - Asia

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

LNP™ THERMOCOMP™ Compound WX15003

Geliefert von:

Sabic