General
Property | Temperature | Value | Comment |
---|---|---|---|
Limiting oxygen index | 23.0 °C | 39 % Show Supplier Material materials with Limiting oxygen index of 39 % | |
Relative density | 23.0 °C | 1.13 [-] Show Supplier Material materials with Relative density of 1.13 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 0.08 % Show Supplier Material materials with Water absorption of 0.08 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastic modulus of 2.6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3.2 % Show Supplier Material materials with Elongation of 3.2 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 87 MPa Show Supplier Material materials with Flexural strength of 87 MPa | ISO 178 | yield, 2 mm/min |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D 785 |
Impact strength, Charpy notched | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | ISO 179/2C | 23°C |
Impact strength, Izod notched | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 20 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 293 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 293 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 720 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 720 J/m | ASTM D 4812 | 23°C |
Taber Abrasion | 23.0 °C | 76 mg/1000cy Show Supplier Material materials with Taber Abrasion of 76 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Tensile strength | 23.0 °C | 58 MPa Show Supplier Material materials with Tensile strength of 58 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature | 82 - 95 °C Show Supplier Material materials with Heat deflection temperature of 82 - 95 °C | ||||
Heat deflection temperature, 0.45 MPa | 95 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 95 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 95 °C Show Supplier Material materials with Relative temperature index, electrical of 95 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 95 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 95 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 0.24 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.24 W/(m·K) | ASTM C177 | ||
Vicat softening temperature | 107 °C Show Supplier Material materials with Vicat softening temperature of 107 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥1mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> Glow Wire Ignitability Temperature, 1.0 mm: 800°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100110155- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 1 V Show Supplier Material materials with Comparative tracking index of 1 V | UL 746A | (UL) {PLC} |
Dielectric constant, 100Hz | 23.0 °C | 2.74 [-] Show Supplier Material materials with Dielectric constant, 100Hz of 2.74 [-] | ASTM D 150 |
Dielectric constant, 1KHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 1KHz of 2.6 [-] | ASTM D 150 |
Dielectric strength | 23.0 °C | 19.2 kV/mm Show Supplier Material materials with Dielectric strength of 19.2 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Dissipation factor, 100Hz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 0.01 [-] | ASTM D 150 |
Dissipation factor, 100kHz | 23.0 °C | 5.5E-3 [-] Show Supplier Material materials with Dissipation factor, 100kHz of 5.5E-3 [-] | ASTM D 150 |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 6 mm Show Supplier Material materials with Hot-Wire Ignition of 6 mm | ≥, UL 746A | PLC 1 |
Volume resistivity | 23.0 °C | 1.80E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.80E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 19.3 g/10min Show Supplier Material materials with Melt mass-flow rate of 19.3 g/10min | ASTM D 1238 | 250°C/10.0 kgf | |
Melt volume-flow rate | 23 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 23 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Vending Machine, Swimming Pool/Spa, Wireless Communications, Wiring Devices, Wearables, Laser Sintering, Power Manangement, Photovoltaic Components, Plumbing, Photo/Video Camera, Servingware, Small Appliance, Surgical Devices, Security/Detection, Respiratory, Monitoring and Imaging, Meter Water, Medical Facility Infrastructure, LED Lighting, Medical Device, Personal Computing, Personal Care, Non-LED Lighting, Document Handling, Door Handle, Displays, Data Transfer, Data Management, Algae, Building Element, Circuit Protection, Audio, Air Conditioning, Electronic Components, Enclosures, Energy Management, Electronics, Enclosure/Housing/Cover, Lab Ware and Clinical Diagnostics, Heavy Vehicles, Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Rear - Zone 1 Temperature: 215 to 265.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |