Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-5 Grade P420ML1 thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
7000 Serie
EN 573-3 Grade AW-7010 T67000 Serie
EN 573-3 Grade AW-7010 T627000 Serie
EN 573-3 Grade AW-7010 T6517000 Serie
EN 573-3 Grade AW-7010 T6527000 Serie
EN 573-3 Grade AW-7010 T7451Duplex rostfreier Stahl
EN 10028-7 Grade X2CrNiMoN22-5-3 solution annealed (+AT)Austenitischer rostfreier Stahl
SEW 400 Grade X2CrNiMnMoNbN25-18-5-4 quenched (+Q)Duplex rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN22-5-3 solution annealed (+AT)Duplex rostfreier Stahl
DIN 5512-3 Grade X2CrNiMoN22-5-3 solution annealed (+AT)