Streckgrenze Rp0,5: 124 - 172 MPa

Quick Comparison

Cast Copper Brass Yellow Brass

ASTM B505 Grade C86500

Geliefert von:

1 Matmatch-Lieferant

Tin Bronze

ASTM B505 Grade C90700

Geliefert von:

1 Matmatch-Lieferant

Leaded Tin Bronze

ASTM B505 Grade C92700

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Brass Yellow Brass

ASTM B584 Grade C86400

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Brass Yellow Brass

ASTM B30 Grade C86400

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Brass Yellow Brass

ASTM B176 Grade C86500

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Silicon Brass

ASTM B584 Grade C87400

Cast Copper Silicon Brass

ASTM B584 Grade C87300

Cast Copper Silicon Brass

ASTM B584 Grade C87500

Cast Copper Silicon Brass

ASTM B584 Grade C87610

Copper Bismuth Alloy

ASTM B505 Grade C89320

Cast Copper Nickel Silver Grade

ASTM B505 Grade C97600

Cast Copper Nickel Silver Grade

ASTM B505 Grade C97800

Cast Copper Nickel Silver Grade

ASTM B271 Grade C97800 As-Cast

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14500 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14510 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14520 H04

Wrought Copper Pure / Low Alloyed Copper

ASTM B301 Grade C14700 H04

Cast Copper Brass Yellow Brass

ASTM B271 Grade C86400 As-Cast