General
Property | Value | Comment |
---|---|---|
Density | 8.47 g/cm³ Show Material materials with Density of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastic modulus | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass | ||
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass | ||
Tensile strength | 448 MPa Show Material materials with Tensile strength of 448 MPa | ASTM B584 | Casting | |
483 MPa Show Material materials with Tensile strength of 483 MPa | ASTM B505 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.5e-05 - 1.9e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.5e-05 - 1.9e-05 1/K | Typical for Cast Copper Brass Yellow Brass |
Melting point | 905 - 932 °C Show Material materials with Melting point of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Specific heat capacity | 335 - 390 J/(kg·K) Show Material materials with Specific heat capacity of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Thermal conductivity | 116 W/(m·K) Show Material materials with Thermal conductivity of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.5 - 1.5 % Show Material materials with Aluminium of 0.5 - 1.5 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Copper | 55 - 60 % Show Material materials with Copper of 55 - 60 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Iron | 0.4 - 2 % Show Material materials with Iron of 0.4 - 2 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Lead | 0.3 % Show Material materials with Lead of 0.3 % | ASTM B30 | |
0.4 % Show Material materials with Lead of 0.4 % | ASTM B176, ASTM B505, ASTM B584 | Casting | |
Manganese | 0.1 - 1.5 % Show Material materials with Manganese of 0.1 - 1.5 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Nickel | 0.8 % Show Material materials with Nickel of 0.8 % | ASTM B30 | |
1 % Show Material materials with Nickel of 1 % | ASTM B176, ASTM B505, ASTM B584 | Casting | |
Tin | 1 % Show Material materials with Tin of 1 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |
Zinc | 36 - 42 % Show Material materials with Zinc of 36 - 42 % | ASTM B176, ASTM B30, ASTM B505, ASTM B584 | Casting |