Austenitischer rostfreier Stahl
EN 10028-7 Grade X2CrNi19-11 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiTi18-10 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X2CrNi19-11 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X2CrNi19-11 quenched (+Q)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNi19-11 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNi18-9 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X2CrNi18-9 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X2CrNi19-11 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNiTi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X2CrNi18-9 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10217-7 Grade X2CrNi19-11 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10217-7 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10217-7 Grade X6CrNiTi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10217-7 Grade X2CrNi18-9 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10250-4 Grade X2CrNi19-11 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10250-4 Grade X2CrNi18-9 solution annealed (+AT)Wrought Copper Nickel Grade
EN 1652 Grade CuNi30Mn1Fe H080Wrought Copper Nickel Grade
EN 12163 Grade CuNi30Mn1Fe R340Wrought Copper Nickel Grade
EN 12451 Grade CuNi30Mn1Fe R370