Unclassified Low Alloy Steel
EN 10025-4 Grade S460M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S460ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10028-6 Grade P460Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P460QH quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10297-1 Grade 36Mn4 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10277-2 Grade St52-3 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade ZSt52-3 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade St 50-2 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade St 60-2 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade St 70-2 cold drawn