CA10 - CuAl7Si2 - C64200

Want to keep this datasheet? Save it now in your required format

Description

Silicon aluminium bronze alloy with good corrosion resistance and machining properties coupled with low magnetic permeability.

Related Standards

Equivalent Materials

This material data has been provided by Lebronze Alloys.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.8 g/cm³

Show Supplier Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

124 GPa

Show Supplier Material materials with Elastic modulus of 124 GPa

Elongation

23.0 °C

30 - 40 %

Show Supplier Material materials with Elongation of 30 - 40 %

Hardness, Brinell

23.0 °C

160 - 210 [-]

Show Supplier Material materials with Hardness, Brinell of 160 - 210 [-]

Hardness, Rockwell C

23.0 °C

3 - 17 [-]

Show Supplier Material materials with Hardness, Rockwell C of 3 - 17 [-]

Hardness, Vickers

23.0 °C

160 - 210 [-]

Show Supplier Material materials with Hardness, Vickers of 160 - 210 [-]

Tensile strength

23.0 °C

570 - 670 MPa

Show Supplier Material materials with Tensile strength of 570 - 670 MPa

Yield strength

23.0 °C

300 - 550 MPa

Show Supplier Material materials with Yield strength of 300 - 550 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

for 20-200°C

Thermal conductivity

23.0 °C

45 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 45 W/(m·K)

for 20-200°C

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

5.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 5.00E+6 S/m

Magnetic

PropertyTemperatureValueComment

Relative magnetic permeability

23.0 °C

1.01 [-]

Show Supplier Material materials with Relative magnetic permeability of 1.01 [-]

max

Technological properties

Property
Application areas

Summary of typical applications: Cryogenic fittings, electrical connectors, rods and couplings, food industry, bolts, valves

Corrosion properties

Corrosion resistance rating: 4 out of 5

Friction

Friction behavior rating: 4 out of 5

General machinability

Machinability: 60 %