Martensitischer Edelstahl
SEW 400 Grade X4CrNi13-4 quenched and tempered (+QT1)Martensitischer Edelstahl
EN 10272 Grade X3CrNiMo13-4 quenched and tempered (+QT780)Martensitischer Edelstahl
EN 10272 Grade X3CrNiMo13-4 quenched and tempered (+QT650)Martensitischer Edelstahl
EN 10250-4 Grade X3CrNiMo13-4 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10028-7 Grade X3CrNiMo13-4 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10222-5 Grade X3CrNiMo13-4 quenched and double tempered (+QT+T)Martensitischer Edelstahl
EN 10213 Grade GX4CrNi13-4 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10250-4 Grade X3CrNiMo13-4 soft annealed (+A)Martensitischer Edelstahl
EN 10088-1 Grade X3CrNiMo13-4 quenched and tempered (+QT650)Martensitischer Edelstahl
ASTM A182 Grade F6NM Normalized and TemperedMartensitischer Edelstahl
ASTM A487 Grade CA6NM Class B, Heat-TreatedMartensitischer Edelstahl
ASTM A352 Grade CA6NM Normalized and Tempered or Liquid Quenched and TemperedMartensitischer Edelstahl
ASTM A356 Grade CA6NM Normalized and Tempered and Stress RelievedMartensitischer Edelstahl
ASTM A743 Grade CA6NM Heat-TreatedMartensitischer Edelstahl
ASTM A336 Grade F6NM Annealed or Normalized and TemperedMartensitischer Edelstahl
SEW 520 Grade GX4CrNi13-4Martensitischer Edelstahl
ASTM A487 Grade CA6NM Class A, Heat-TreatedMartensitischer Edelstahl
JIS G3214 Grade SUSF6NMMartensitischer Edelstahl
JIS G5121 Grade SCS5Martensitischer Edelstahl
JIS G5121 Grade SCS6