Martensitischer Edelstahl
SEW 400 Grade X4CrNi13-4 quenched and tempered (+QT1)Martensitischer Edelstahl
EN 10272 Grade X3CrNiMo13-4 quenched and tempered (+QT780)Martensitischer Edelstahl
EN 10272 Grade X3CrNiMo13-4 quenched and tempered (+QT650)Martensitischer Edelstahl
EN 10250-4 Grade X3CrNiMo13-4 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10028-7 Grade X3CrNiMo13-4 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10222-5 Grade X3CrNiMo13-4 quenched and double tempered (+QT+T)Martensitischer Edelstahl
DIN 17445 Grade G-X5CrNi13-4 quenched and tempered (+QT1)Martensitischer Edelstahl
EN 10250-4 Grade X3CrNiMo13-4 soft annealed (+A)Martensitischer Edelstahl
EN 10088-1 Grade X3CrNiMo13-4 quenched and tempered (+QT650)Martensitischer Edelstahl
ASTM A182 Grade F6NM Normalized and TemperedMartensitischer Edelstahl
ASTM A240 Grade S41500 Heat-TreatedMartensitischer Edelstahl
ASTM A276 Grade S41500 Hardened and tempered at a relatively high temperature; Hot-Finished or Cold-FinishedMartensitischer Edelstahl
ASTM A268 Grade S41500 ReheatedMartensitischer Edelstahl
ASTM A487 Grade CA6NM Class B, Heat-TreatedMartensitischer Edelstahl
ASTM A473 Grade S41500 Normalized and temperedMartensitischer Edelstahl
ASTM A352 Grade CA6NM Normalized and Tempered or Liquid Quenched and Tempered