Wrought Copper Pure / Low Alloyed Copper
CEN/TS 13388 Grade CW016A MWrought Copper Pure / Low Alloyed Copper
ASTM B888 Grade C15500 H02Wrought Copper Pure / Low Alloyed Copper
ASTM B888 Grade C15500 H04Wrought Copper Pure / Low Alloyed Copper
ASTM B888 Grade C15500 H06Wrought Copper Pure / Low Alloyed Copper
ASTM B888 Grade C15500 H08Wrought Copper Pure / Low Alloyed Copper
ASTM B888 Grade C15500 H10Wrought Copper Pure / Low Alloyed Copper
ASTM B888 Grade C15500 O61Wrought Copper Pure / Low Alloyed Copper
EN 1976 Grade CR016AWrought Copper Pure / Low Alloyed Copper
DIN 17666 Grade CW016AWrought Copper Pure / Low Alloyed Copper
NP 3634 Grade CW016AWrought Copper Pure / Low Alloyed Copper
UNE 37-137 Grade CW016AWrought Copper Pure / Low Alloyed Copper
ÖNORM M 3403 Grade CW016AWrought Copper Pure / Low Alloyed Copper
SN 211600 Grade CW016AWrought Copper Pure / Low Alloyed Copper
UNI 5649-2 Grade CW016AWrought Copper Pure / Low Alloyed Copper
ISO 1336 Grade CuAg0,1(P)