ASTM B888 Grade C15500 H06

View suppliers (1)
Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Typical for Wrought Copper Pure / Low Alloyed Copper

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

95 - 98 GPa

Show Material materials with Elastic modulus of 95 - 98 GPa

Typical for Wrought Copper Pure / Low Alloyed Copper

Elongation

23.0 °C

5 %

Show Material materials with Elongation of 5 %

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Typical for Wrought Copper Pure / Low Alloyed Copper

Shear modulus

23.0 °C

48 GPa

Show Material materials with Shear modulus of 48 GPa

Typical for Wrought Copper Pure / Low Alloyed Copper

Tensile strength

23.0 °C

435 - 495 MPa

Show Material materials with Tensile strength of 435 - 495 MPa

Yield strength Rp0.2

23.0 °C

385 MPa

Show Material materials with Yield strength Rp0.2 of 385 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K

Typical for Wrought Copper Pure / Low Alloyed Copper

Melting point

965 - 1100 °C

Show Material materials with Melting point of 965 - 1100 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Specific heat capacity

23.0 °C

377 - 420 J/(kg·K)

Show Material materials with Specific heat capacity of 377 - 420 J/(kg·K)

Typical for Wrought Copper Pure / Low Alloyed Copper

Chemical properties

PropertyValue

Copper

99.75 %

Show Material materials with Copper of 99.75 %

Magnesium

0.08 - 0.13 %

Show Material materials with Magnesium of 0.08 - 0.13 %

Phosphorus

0.04 - 0.08 %

Show Material materials with Phosphorus of 0.04 - 0.08 %

Silver

0.03 - 0.1 %

Show Material materials with Silver of 0.03 - 0.1 %