Wrought Copper High Copper Alloy
ASTM B643 Grade C17200 TH04Wrought Copper High Copper Alloy
ASTM B570 Grade C17000 TD02Wrought Copper High Copper Alloy
ASTM B570 Grade C17000 TD01Wrought Copper High Copper Alloy
Alloy 25 Forging, Extrusion TB00 (C17200)Geliefert von:
Materion Brush GmbHWrought Copper High Copper Alloy
Alloy 25 Forging, Extrusion TF00 (C17200)Geliefert von:
Materion Brush GmbHWrought Copper High Copper Alloy
Alloy 165 Forging, Extrusion TB00 (C17000)Geliefert von:
Materion Brush GmbHWrought Copper High Copper Alloy
Alloy 165 Forging, Extrusion TF00 (C17000)Geliefert von:
Materion Brush GmbHWrought Copper High Copper Alloy
ASTM B570 Grade C17000 TF00Wrought Copper High Copper Alloy
ASTM B570 Grade C17200 TF00Wrought Copper High Copper Alloy
ASTM B570 Grade C17000 TB00Wrought Copper High Copper Alloy
ASTM B570 Grade C17200 TB00