EN 10028-4

Quick Comparison

Nickel Steel

EN 10028-4 Grade X12Ni5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 11MnNi5-3 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 13MnNi6-3 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 15NiMn6 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade X8Ni9 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade X8Ni9 normalized, normalized and tempered (+N+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade X8Ni9 normalized or quenched and tempered

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade X7Ni9 normalized, normalized and tempered (+N+NT)

Geliefert von:

1 Matmatch-Lieferant