Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | T4 | EN 573-3, EN 1301, EN 1715-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 180° | 3.0 °/t Show Material materials with Biegewinkel 180° of 3.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
Biegewinkel 90° | 1.5 °/t Show Material materials with Biegewinkel 90° of 1.5 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
2.0 °/t Show Material materials with Biegewinkel 90° of 2.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
3.0 °/t Show Material materials with Biegewinkel 90° of 3.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
4.0 °/t Show Material materials with Biegewinkel 90° of 4.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
Dehnung | 13.0 % Show Material materials with Dehnung of 13.0 % | T4 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar | ||
14.0 % Show Material materials with Dehnung of 14.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
15.0 % Show Material materials with Dehnung of 15.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
15.0 % Show Material materials with Dehnung of 15.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
16.0 % Show Material materials with Dehnung of 16.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
18.0 % Show Material materials with Dehnung of 18.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
20.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | T4 | EN 573-3 | Profile, Rod | A50 | |
20.0 °C | 15.0 % Show Material materials with Dehnung of 15.0 % | T4 | EN 573-3 | Profile, Rod | ||
20.0 °C | 15.0 % Show Material materials with Dehnung of 15.0 % | T4 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 16.0 % Show Material materials with Dehnung of 16.0 % | T4 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 18.0 % Show Material materials with Dehnung of 18.0 % | T4 | EN 573-3 | Flat | A50 Transverse | |
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Härte, Brinell | 78.0 [-] Show Material materials with Härte, Brinell of 78.0 [-] | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
95.0 [-] Show Material materials with Härte, Brinell of 95.0 [-] | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 78.0 [-] Show Material materials with Härte, Brinell of 78.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 95.0 [-] Show Material materials with Härte, Brinell of 95.0 [-] | T4 | EN 573-3 | Profile, Rod | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Zugfestigkeit | 265.0 MPa Show Material materials with Zugfestigkeit of 265.0 MPa | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
300.0 - 380.0 MPa Show Material materials with Zugfestigkeit of 300.0 - 380.0 MPa | T4 | EN 573-3, EN 1301, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |||
350.0 MPa Show Material materials with Zugfestigkeit of 350.0 MPa | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 265.0 MPa Show Material materials with Zugfestigkeit of 265.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 350.0 MPa Show Material materials with Zugfestigkeit of 350.0 MPa | T4 | EN 573-3 | Profile, Rod |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 6000 Series Aluminium |
Schmelzpunkt | 555.0 - 655.0 °C Show Material materials with Schmelzpunkt of 555.0 - 655.0 °C | Typical for Wrought 6000 Series Aluminium |
Spezifische Wärmekapazität | 887.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium |
Wärmeleitfähigkeit | 170.0 - 220.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 170.0 - 220.0 W/(m·K) | Typical for Wrought 6000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 21000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 21000000.0 - 34000000.0 S/m | Typical for Wrought 6000 Series Aluminium |
spezifischer Widerstand | 2.9e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | T4 | EN 573-3, EN 1301, EN 1715-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | T4 | EN 573-3 | Profile, Rod, Flat |
0.50 % Show Material materials with Eisen of 0.50 % | T4 | EN 573-3, EN 1301, EN 1715-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | |
Kupfer | 0.5 - 1.1 % Show Material materials with Kupfer of 0.5 - 1.1 % | T4 | EN 573-3, EN 1301, EN 1715-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Magnesium | 0.6 - 1.2 % Show Material materials with Magnesium of 0.6 - 1.2 % | T4 | EN 573-3, EN 1301, EN 1715-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Mangan | 0.4 - 1.0 % Show Material materials with Mangan of 0.4 - 1.0 % | T4 | EN 573-3, EN 1301, EN 1715-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Silizium | 0.7 - 1.3 % Show Material materials with Silizium of 0.7 - 1.3 % | T4 | EN 573-3, EN 1301, EN 1715-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Zink | 0.1 - 0.7 % Show Material materials with Zink of 0.1 - 0.7 % | T4 | EN 573-3, EN 1301, EN 1715-3, EN 485, EN 755 | Profile, Rod, Flat, Strip, Sheet, Plate, Tube, Bar |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |