we have enjoyed a first-rate reputation as a manufacturer of aluminium profiles, aluminium discs as a primary material for cold forming processes (slugs) and mechanically processed extruded products.
Headquarters
Wutöschingen, Germany
Website
Type
Manufacturer and Processor
Certifications
ISO 9001
, IATF 16949
Grade | Shape | ||
---|---|---|---|
EN AW-1050A | Profile, Extrusion | EN AW-1050A, DIN Al99.5 | EN 573-3 |
EN AW-1070A | Profile, Extrusion | EN AW-1070A, DIN Al99.7 | EN 573-3 |
EN AW-1100 | Profile, Extrusion | EN AW-1100, DIN Al99.0Cu | EN 573-3 |
EN AW-1350A | Profile, Extrusion | EN AW-1350A | EN 573-3 |
EN AW-3003 | Profile, Extrusion | EN AW-3003, DIN AlMn1Cu | EN 573-3 |
EN AW-3004 | Profile, Extrusion | EN AW-3004, DIN AlMn1Mg1 | EN 573-3 |
EN AW-3102 | Profile, Extrusion | EN AW-3102, DIN AlMn0.2 | EN 573-3 |
EN AW-3103 | Profile, Extrusion | EN AW-3103, DIN AlMn1 | EN 573-3 |
EN AW-5005A | Profile, Extrusion | EN AW-5005A, DIN AlMg1(C) | EN 573-3 |
EN AW-5210 | Profile, Extrusion | EN AW-5210, DIN Al99.9Mg0.5 | EN 573-3 |