Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.78 g/cm³ Show Material materials with Dichte of 2.78 g/cm³ | T6 | EN 573-3, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Tube | |
20.0 °C | 2.78 g/cm³ Show Material materials with Dichte of 2.78 g/cm³ | T6 | EN 573-3 | Profile, Rod, Flat, Tube, Sheet |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 3.0 % Show Material materials with Dehnung of 3.0 % | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube | A100 | |
5.0 % Show Material materials with Dehnung of 5.0 % | T6 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Tube | A50 | ||
5.0 % Show Material materials with Dehnung of 5.0 % | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube | A100 | ||
6.0 % Show Material materials with Dehnung of 6.0 % | T6 | EN 573-3, EN 754 | Strip, Sheet, Plate, Rod, Tube | A50 | ||
7.0 % Show Material materials with Dehnung of 7.0 % | T6 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Rod, Tube | A100 | ||
8.0 % Show Material materials with Dehnung of 8.0 % | T6 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Rod, Tube | A50 | ||
8.0 % Show Material materials with Dehnung of 8.0 % | T6 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Rod, Tube | A100 | ||
20.0 °C | 3.0 % Show Material materials with Dehnung of 3.0 % | T6 | EN 573-3 | Sheet | ||
20.0 °C | 3.0 % Show Material materials with Dehnung of 3.0 % | T6 | EN 573-3 | Flat | Transverse | |
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T6 | EN 573-3 | Profile, Rod, Tube | A50 | |
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T6 | EN 573-3 | Sheet | ||
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | T6 | EN 573-3 | Flat | Transverse | |
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T6 | EN 573-3 | Rod, Tube | A50 | |
20.0 °C | 7.0 % Show Material materials with Dehnung of 7.0 % | T6 | EN 573-3 | Profile, Tube, Rod, Sheet | ||
20.0 °C | 7.0 % Show Material materials with Dehnung of 7.0 % | T6 | EN 573-3 | Flat | Transverse | |
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T6 | EN 573-3 | Flat | A50 | |
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T6 | EN 573-3 | Rod, Tube, Flat | ||
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T6 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T6 | EN 573-3 | Flat | Transverse | |
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | T6 | EN 573-3, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Tube | ||
20.0 °C | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | T6 | EN 573-3 | Profile, Rod, Flat, Tube, Sheet | ||
Härte, Brinell | 121.0 [-] Show Material materials with Härte, Brinell of 121.0 [-] | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube | ||
127.0 [-] Show Material materials with Härte, Brinell of 127.0 [-] | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube | |||
133.0 [-] Show Material materials with Härte, Brinell of 133.0 [-] | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube | |||
20.0 °C | 121.0 - 133.0 [-] Show Material materials with Härte, Brinell of 121.0 - 133.0 [-] | T6 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 121.0 - 127.0 [-] Show Material materials with Härte, Brinell of 121.0 - 127.0 [-] | T6 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 121.0 [-] Show Material materials with Härte, Brinell of 121.0 [-] | T6 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 127.0 - 133.0 [-] Show Material materials with Härte, Brinell of 127.0 - 133.0 [-] | T6 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 127.0 [-] Show Material materials with Härte, Brinell of 127.0 [-] | T6 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 133.0 [-] Show Material materials with Härte, Brinell of 133.0 [-] | T6 | EN 573-3 | Profile, Rod, Tube, Flat, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Schubmodule | 20.0 °C | 27.5 GPa Show Material materials with Schubmodule of 27.5 GPa | T6 | EN 573-3 | Profile, Rod, Flat, Tube, Sheet | |
Zugfestigkeit | 410.0 MPa Show Material materials with Zugfestigkeit of 410.0 MPa | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube | ||
430.0 MPa Show Material materials with Zugfestigkeit of 430.0 MPa | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube | |||
450.0 MPa Show Material materials with Zugfestigkeit of 450.0 MPa | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube | |||
460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T6 | EN 573-3, EN 754 | Strip, Sheet, Plate, Rod, Tube | |||
470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T6 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Tube | |||
490.0 MPa Show Material materials with Zugfestigkeit of 490.0 MPa | T6 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Tube | |||
20.0 °C | 410.0 MPa Show Material materials with Zugfestigkeit of 410.0 MPa | T6 | EN 573-3 | Sheet | ||
20.0 °C | 410.0 MPa Show Material materials with Zugfestigkeit of 410.0 MPa | T6 | EN 573-3 | Flat | Transverse | |
20.0 °C | 430.0 MPa Show Material materials with Zugfestigkeit of 430.0 MPa | T6 | EN 573-3 | Sheet | ||
20.0 °C | 430.0 MPa Show Material materials with Zugfestigkeit of 430.0 MPa | T6 | EN 573-3 | Flat | Transverse | |
20.0 °C | 450.0 MPa Show Material materials with Zugfestigkeit of 450.0 MPa | T6 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 450.0 MPa Show Material materials with Zugfestigkeit of 450.0 MPa | T6 | EN 573-3 | Flat | Transverse | |
20.0 °C | 460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T6 | EN 573-3 | Rod, Tube | ||
20.0 °C | 470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T6 | EN 573-3 | Rod | ||
20.0 °C | 490.0 MPa Show Material materials with Zugfestigkeit of 490.0 MPa | T6 | EN 573-3 | Profile, Rod, Tube |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | T6 | EN 573-3, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Tube | |
100 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | T6 | EN 573-3, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Tube | ||
Schmelzpunkt | 480.0 - 640.0 °C Show Material materials with Schmelzpunkt of 480.0 - 640.0 °C | T6 | EN 573-3, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Tube | ||
Spezifische Wärmekapazität | 795.0 - 1050.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium | ||||
Wärmeleitfähigkeit | 20.0 °C | 130.0 - 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 160.0 W/(m·K) | T6 | EN 573-3, EN 485, EN 754, EN 755 | Profile, Rod, Flat, Tube, Sheet, Strip, Plate |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 19000000.0 - 23000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 19000000.0 - 23000000.0 S/m | T6 | EN 573-3, EN 485, EN 754, EN 755 | Profile, Rod, Flat, Tube, Sheet, Strip, Plate |
spezifischer Widerstand | 4.35e-08 - 5.26e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.35e-08 - 5.26e-08 Ω·m | T6 | EN 573-3, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 - 0.3 % Show Material materials with Chrom of 0.1 - 0.3 % | T6 | EN 573-3, EN 485, EN 754, EN 755 | Profile, Rod, Flat, Tube, Sheet, Strip, Plate |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | T6 | EN 573-3 | Profile, Rod, Flat, Tube, Sheet |
0.50 % Show Material materials with Eisen of 0.50 % | T6 | EN 573-3, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Tube | |
Kupfer | 0.5 - 1.0 % Show Material materials with Kupfer of 0.5 - 1.0 % | T6 | EN 573-3, EN 485, EN 754, EN 755 | Profile, Rod, Flat, Tube, Sheet, Strip, Plate |
Magnesium | 2.6 - 3.7 % Show Material materials with Magnesium of 2.6 - 3.7 % | T6 | EN 573-3, EN 485, EN 754, EN 755 | Profile, Rod, Flat, Tube, Sheet, Strip, Plate |
Mangan | 0.1 - 0.4 % Show Material materials with Mangan of 0.1 - 0.4 % | T6 | EN 573-3, EN 485, EN 754, EN 755 | Profile, Rod, Flat, Tube, Sheet, Strip, Plate |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | T6 | EN 573-3, EN 485, EN 754, EN 755 | Profile, Rod, Flat, Tube, Sheet, Strip, Plate |
Zink | 4.3 - 5.2 % Show Material materials with Zink of 4.3 - 5.2 % | T6 | EN 573-3, EN 485, EN 754, EN 755 | Profile, Rod, Flat, Tube, Sheet, Strip, Plate |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not suitable, Protective: good | |
Brazing | hard brazing (with flux/ without flux): not suitable / not suitable, friction soldering: not suitable, soft brazing with flux: not suitable | |
Corrosion properties | Seawater: poor, weathering: sufficient | |
Workability | Bending / Spinning (cold): poor (O) / not suitable, Impact extrusion (cold): not suitable, Deep drawing / upsetting (Condition) not suitable / not suitable |