The GLEICH Group is a traditional family owned company from Kaltenkirchen, close to Hamburg. Founded in 1980 by Günter and Christel Gleich, the group of companies is now run by the second generation, headed by Roland Gleich. The core business since the mid-1990s has been the development, production and worldwide distribution of G.AL® aluminum plates. The brand name G.AL® stands for extremely low-distortion, dimensionally-stable and homogeneous aluminum precision and mould plates of consistently high quality.
Webseite
Umsatz
1-100M USD
Anzahl der Mitarbeiter
1-250
Gründungsjahr
1980
Art
Hersteller und Händler
Zusätzlich: Aluminium Cast Plates, Aluminium Rolled Plates, Aluminium Round Bars