Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | EN 573-3 | Strip, Sheet, Plate |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 68.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 68.0 - 70.0 GPa | Typical for Wrought 1000 Series Aluminium |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium |
Schubmodule | 25.9 GPa Show Material materials with Schubmodule of 25.9 GPa | Typical for Wrought 1000 Series Aluminium |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.2e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 1000 Series Aluminium |
Schmelzpunkt | 645.0 - 660.0 °C Show Material materials with Schmelzpunkt of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium |
Spezifische Wärmekapazität | 900.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium |
Wärmeleitfähigkeit | 167.0 - 244.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 167.0 - 244.0 W/(m·K) | Typical for Wrought 1000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 33000000.0 - 38000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
spezifischer Widerstand | 2.7e-08 - 3e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 99.85 % Show Material materials with Aluminium of 99.85 % | EN 573-3 | Strip, Sheet, Plate |
Eisen | 0.12 % Show Material materials with Eisen of 0.12 % | EN 573-3 | |
0.12 % Show Material materials with Eisen of 0.12 % | EN 573-3 | Strip, Sheet, Plate | |
Gallium | 0.03 % Show Material materials with Gallium of 0.03 % | EN 573-3 | Strip, Sheet, Plate |
Kupfer | 0.03 % Show Material materials with Kupfer of 0.03 % | EN 573-3 | Strip, Sheet, Plate |
Magnesium | 0.02 % Show Material materials with Magnesium of 0.02 % | EN 573-3 | Strip, Sheet, Plate |
Mangan | 0.02 % Show Material materials with Mangan of 0.02 % | EN 573-3 | Strip, Sheet, Plate |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % | EN 573-3 | Strip, Sheet, Plate |
Titan | 0.02 % Show Material materials with Titan of 0.02 % | EN 573-3 | Strip, Sheet, Plate |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % | EN 573-3 | Strip, Sheet, Plate |
Zink | 0.03 % Show Material materials with Zink of 0.03 % | EN 573-3 | Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |