Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 180° | 3.0 °/t Show Material materials with Biegewinkel 180° of 3.0 °/t | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
5.0 °/t Show Material materials with Biegewinkel 180° of 5.0 °/t | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
Biegewinkel 90° | 3.0 °/t Show Material materials with Biegewinkel 90° of 3.0 °/t | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
5.0 °/t Show Material materials with Biegewinkel 90° of 5.0 °/t | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
8.0 °/t Show Material materials with Biegewinkel 90° of 8.0 °/t | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
Dehnung | 2.0 % Show Material materials with Dehnung of 2.0 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A100 | |
4.0 % Show Material materials with Dehnung of 4.0 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
6.0 % Show Material materials with Dehnung of 6.0 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
7.0 % Show Material materials with Dehnung of 7.0 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
12.0 % Show Material materials with Dehnung of 12.0 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
13.0 % Show Material materials with Dehnung of 13.0 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
14.0 % Show Material materials with Dehnung of 14.0 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
15.0 % Show Material materials with Dehnung of 15.0 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | T451 | EN 573-3 | Sheet | ||
20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | T451 | EN 573-3 | Sheet | ||
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T451 | EN 573-3 | Sheet | ||
20.0 °C | 6.0 % Show Material materials with Dehnung of 6.0 % | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 7.0 % Show Material materials with Dehnung of 7.0 % | T451 | EN 573-3 | Sheet | ||
20.0 °C | 7.0 % Show Material materials with Dehnung of 7.0 % | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 12.0 % Show Material materials with Dehnung of 12.0 % | T451 | EN 573-3 | Flat, Sheet | ||
20.0 °C | 12.0 % Show Material materials with Dehnung of 12.0 % | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 13.0 % Show Material materials with Dehnung of 13.0 % | T451 | EN 573-3 | Flat | A50 | |
20.0 °C | 13.0 % Show Material materials with Dehnung of 13.0 % | T451 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | T451 | EN 573-3 | Flat | A50 | |
20.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | T451 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 15.0 % Show Material materials with Dehnung of 15.0 % | T451 | EN 573-3 | Flat | A50 | |
20.0 °C | 15.0 % Show Material materials with Dehnung of 15.0 % | T451 | EN 573-3 | Flat | A50 Transverse | |
Elastizitätsmodul | 72.5 GPa Show Material materials with Elastizitätsmodul of 72.5 GPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
20.0 °C | 65.0 - 73.5 GPa Show Material materials with Elastizitätsmodul of 65.0 - 73.5 GPa | T451 | EN 573-3 | Flat, Sheet | ||
Härte, Brinell | 101.0 [-] Show Material materials with Härte, Brinell of 101.0 [-] | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
105.0 [-] Show Material materials with Härte, Brinell of 105.0 [-] | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
108.0 [-] Show Material materials with Härte, Brinell of 108.0 [-] | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
110.0 [-] Show Material materials with Härte, Brinell of 110.0 [-] | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
111.0 [-] Show Material materials with Härte, Brinell of 111.0 [-] | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 101.0 - 108.0 [-] Show Material materials with Härte, Brinell of 101.0 - 108.0 [-] | T451 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 101.0 - 105.0 [-] Show Material materials with Härte, Brinell of 101.0 - 105.0 [-] | T451 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 101.0 [-] Show Material materials with Härte, Brinell of 101.0 [-] | T451 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 101.0 - 110.0 [-] Show Material materials with Härte, Brinell of 101.0 - 110.0 [-] | T451 | EN 573-3 | Flat | ||
20.0 °C | 101.0 - 111.0 [-] Show Material materials with Härte, Brinell of 101.0 - 111.0 [-] | T451 | EN 573-3 | Flat | ||
20.0 °C | 105.0 - 108.0 [-] Show Material materials with Härte, Brinell of 105.0 - 108.0 [-] | T451 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 105.0 [-] Show Material materials with Härte, Brinell of 105.0 [-] | T451 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 105.0 - 110.0 [-] Show Material materials with Härte, Brinell of 105.0 - 110.0 [-] | T451 | EN 573-3 | Flat | ||
20.0 °C | 105.0 - 111.0 [-] Show Material materials with Härte, Brinell of 105.0 - 111.0 [-] | T451 | EN 573-3 | Flat | ||
20.0 °C | 108.0 [-] Show Material materials with Härte, Brinell of 108.0 [-] | T451 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 108.0 - 110.0 [-] Show Material materials with Härte, Brinell of 108.0 - 110.0 [-] | T451 | EN 573-3 | Flat | ||
20.0 °C | 108.0 - 111.0 [-] Show Material materials with Härte, Brinell of 108.0 - 111.0 [-] | T451 | EN 573-3 | Flat | ||
20.0 °C | 110.0 [-] Show Material materials with Härte, Brinell of 110.0 [-] | T451 | EN 573-3 | Flat | ||
20.0 °C | 110.0 - 111.0 [-] Show Material materials with Härte, Brinell of 110.0 - 111.0 [-] | T451 | EN 573-3 | Flat | ||
20.0 °C | 111.0 [-] Show Material materials with Härte, Brinell of 111.0 [-] | T451 | EN 573-3 | Flat | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Schubmodule | 27.2 GPa Show Material materials with Schubmodule of 27.2 GPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
20.0 °C | 26.0 - 28.5 GPa Show Material materials with Schubmodule of 26.0 - 28.5 GPa | T451 | EN 573-3 | Flat, Sheet | ||
Zugfestigkeit | 300.0 MPa Show Material materials with Zugfestigkeit of 300.0 MPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
330.0 MPa Show Material materials with Zugfestigkeit of 330.0 MPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
350.0 MPa Show Material materials with Zugfestigkeit of 350.0 MPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
360.0 MPa Show Material materials with Zugfestigkeit of 360.0 MPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
370.0 MPa Show Material materials with Zugfestigkeit of 370.0 MPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
385.0 MPa Show Material materials with Zugfestigkeit of 385.0 MPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
390.0 MPa Show Material materials with Zugfestigkeit of 390.0 MPa | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 300.0 MPa Show Material materials with Zugfestigkeit of 300.0 MPa | T451 | EN 573-3 | Sheet | ||
20.0 °C | 300.0 MPa Show Material materials with Zugfestigkeit of 300.0 MPa | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 330.0 MPa Show Material materials with Zugfestigkeit of 330.0 MPa | T451 | EN 573-3 | Sheet | ||
20.0 °C | 330.0 MPa Show Material materials with Zugfestigkeit of 330.0 MPa | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 350.0 MPa Show Material materials with Zugfestigkeit of 350.0 MPa | T451 | EN 573-3 | Sheet | ||
20.0 °C | 350.0 MPa Show Material materials with Zugfestigkeit of 350.0 MPa | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 360.0 MPa Show Material materials with Zugfestigkeit of 360.0 MPa | T451 | EN 573-3 | Sheet | ||
20.0 °C | 360.0 MPa Show Material materials with Zugfestigkeit of 360.0 MPa | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 370.0 MPa Show Material materials with Zugfestigkeit of 370.0 MPa | T451 | EN 573-3 | Sheet | ||
20.0 °C | 370.0 MPa Show Material materials with Zugfestigkeit of 370.0 MPa | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 385.0 MPa Show Material materials with Zugfestigkeit of 385.0 MPa | T451 | EN 573-3 | Sheet | ||
20.0 °C | 385.0 MPa Show Material materials with Zugfestigkeit of 385.0 MPa | T451 | EN 573-3 | Flat | Transverse | |
20.0 °C | 390.0 MPa Show Material materials with Zugfestigkeit of 390.0 MPa | T451 | EN 573-3 | Flat | ||
20.0 °C | 390.0 MPa Show Material materials with Zugfestigkeit of 390.0 MPa | T451 | EN 573-3 | Flat | Transverse |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar |
100 °C | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |
Schmelzpunkt | 512.0 - 650.0 °C Show Material materials with Schmelzpunkt of 512.0 - 650.0 °C | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |
Spezifische Wärmekapazität | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 921.0 J/(kg·K) | T451 | EN 573-3 | Flat, Sheet |
Wärmeleitfähigkeit | 20.0 °C | 130.0 - 200.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 200.0 W/(m·K) | T451 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate, Tube, Bar |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 18000000.0 - 28000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 28000000.0 S/m | T451 | EN 573-3, EN 485 | Flat, Sheet, Strip, Plate, Tube, Bar |
spezifischer Widerstand | 3.57e-08 - 5.56e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.57e-08 - 5.56e-08 Ω·m | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | T451 | EN 573-3, EN 485 | Sheet, Flat, Strip, Plate, Tube, Bar |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | T451 | EN 573-3 | Sheet, Flat |
0.70 % Show Material materials with Eisen of 0.70 % | T451 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |
Kupfer | 3.5 - 4.5 % Show Material materials with Kupfer of 3.5 - 4.5 % | T451 | EN 573-3, EN 485 | Sheet, Flat, Strip, Plate, Tube, Bar |
Magnesium | 0.4 - 1.0 % Show Material materials with Magnesium of 0.4 - 1.0 % | T451 | EN 573-3, EN 485 | Sheet, Flat, Strip, Plate, Tube, Bar |
Mangan | 0.4 - 1.0 % Show Material materials with Mangan of 0.4 - 1.0 % | T451 | EN 573-3, EN 485 | Sheet, Flat, Strip, Plate, Tube, Bar |
Silizium | 0.2 - 0.8 % Show Material materials with Silizium of 0.2 - 0.8 % | T451 | EN 573-3, EN 485 | Sheet, Flat, Strip, Plate, Tube, Bar |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | T451 | EN 573-3, EN 485 | Sheet, Flat, Strip, Plate, Tube, Bar |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not suitable, Protective: good | |
Brazing | hard brazing (with flux/ without flux): not suitable / not suitable, friction soldering: acceptable, soft brazing with flux: not suitable | |
Corrosion properties | Seawater: poor, weathering: sufficient | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) acceptable (O) / acceptable (O) |