today an outstanding company for the production of special steels, and also provides aluminium bars and titanium wire in coils and bars.
Headquarters
VICENZA, Italy
Website
Type
Manufacturer and Processor
Certifications
ISO 9001
Grade | Shape | ||
---|---|---|---|
EN 1.0302 | Bar | EN 1.0302, DIN C10Pb | |
EN 1.0502 | Bar | EN 1.0502, EN C35Pb | |
EN 1.0503 | Bar | EN 1.0503, EN C45 | |
EN 1.0504 | Bar | EN 1.0504, EN C45Pb | |
EN 1.0540 | Bar | EN 1.0540, EN C50 | |
EN 1.0715 | Bar | EN 1.0715, EN 1.0736, EN 11SMn30, EN 11SMn37 | |
EN 1.0718 | Bar | EN 1.0718, EN 1.0737, EN 11SMnPb30, EN 11SMnPb37 | |
EN 1.0726 | Bar | EN 1.0726, EN 1.0756, EN 35S20, EN 35SPb20 | |
EN 1.0727 | Bar | EN 1.0727, EN 1.0757, EN 45S20, EN 45SPb20 | |
EN 1.0739 | Bar | EN 1.0739, EN 11SMnPb37 | |