Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H19 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Coil, Sheet |
Abmessung
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 180° | 0 °/t Show Material materials with Biegewinkel 180° of 0 °/t | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | ||
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | |||
70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Härte, Brinell | 67.0 [-] Show Material materials with Härte, Brinell of 67.0 [-] | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 67.0 [-] Show Material materials with Härte, Brinell of 67.0 [-] | H19 | EN 573-3 | Flat | ||
Härte, HBW | 67 [-] Show Material materials with Härte, HBW of 67 [-] | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Schubmodule | 26.0 GPa Show Material materials with Schubmodule of 26.0 GPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | ||
Streckgrenze | 190.0 MPa Show Material materials with Streckgrenze of 190.0 MPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | RP02 | |
190 MPa Show Material materials with Streckgrenze of 190 MPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | |||
20.0 °C | 190.0 MPa Show Material materials with Streckgrenze of 190.0 MPa | H19 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 190.0 MPa Show Material materials with Streckgrenze of 190.0 MPa | H19 | EN 573-3 | Flat | RP02 | |
Zugfestigkeit | 215.0 MPa Show Material materials with Zugfestigkeit of 215.0 MPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
215 MPa Show Material materials with Zugfestigkeit of 215 MPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | |||
20.0 °C | 215.0 MPa Show Material materials with Zugfestigkeit of 215.0 MPa | H19 | EN 573-3 | Flat | Transverse | |
20.0 °C | 215.0 MPa Show Material materials with Zugfestigkeit of 215.0 MPa | H19 | EN 573-3 | Flat |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
100 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
100 °C | 0.000024 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000024 1/K | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | 20-100°C | |
Schmelzpunkt | 635.0 - 655.0 °C Show Material materials with Schmelzpunkt of 635.0 - 655.0 °C | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
640.0 - 655.0 °C Show Material materials with Schmelzpunkt of 640.0 - 655.0 °C | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Spezifische Wärmekapazität | 893.0 - 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium | ||||
Wärmeleitfähigkeit | 160.0 - 190.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 160.0 - 190.0 W/(m·K) | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
172 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 172 W/(m·K) | H19 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Strip, Sheet, Plate, Coil, Sheet | |||
20.0 °C | 180.0 - 190.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 180.0 - 190.0 W/(m·K) | H19 | EN 573-3 | Flat |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 26000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 26000000.0 S/m | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
26000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 26000000.0 S/m | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 25000000.0 - 27000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 25000000.0 - 27000000.0 S/m | H19 | EN 573-3 | Flat | |
spezifischer Widerstand | 3.7999999999999996e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.7999999999999996e-08 Ω·m | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | |
3.85e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.85e-08 Ω·m | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
3.85e-08 - 4.35e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.85e-08 - 4.35e-08 Ω·m | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.2 % Show Material materials with Chrom of 0.2 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.2 % Show Material materials with Chrom of 0.2 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | H19 | EN 573-3 | Flat |
0.70 % Show Material materials with Eisen of 0.70 % | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
0.7 % Show Material materials with Eisen of 0.7 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.3 % Show Material materials with Kupfer of 0.3 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | |
Magnesium | 0.2 - 0.8 % Show Material materials with Magnesium of 0.2 - 0.8 % | H19 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Coil, Sheet |
Mangan | 0.3 - 0.8 % Show Material materials with Mangan of 0.3 - 0.8 % | H19 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Coil, Sheet |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.6 % Show Material materials with Silizium of 0.6 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet | |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Zink | 0.4 % Show Material materials with Zink of 0.4 % | H19 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
0.4 % Show Material materials with Zink of 0.4 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Heat exchangers: Fins; Closures: Short cups; Semi-rigid and corrugated: Pet food | |
Brazing | hard brazing (with flux/ without flux): very good - acceptable / very good | |
Corrosion properties | Seawater: very good, weathering: very good | |
Surface Finish | Mill finish | |
Welding | Very Good | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) very good (H14) / acceptable (H12) |