Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | ||
20.0 °C | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Sheet, Strip, Wire |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 60.0 MPa Show Material materials with Bending Fatigue Strength of 60.0 MPa | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | |||
Biegewinkel 180° | 1.0 °/t Show Material materials with Biegewinkel 180° of 1.0 °/t | O | EN 573-3, EN 485 | |||
Biegewinkel 90° | 0.5 °/t Show Material materials with Biegewinkel 90° of 0.5 °/t | O | EN 573-3, EN 485 | |||
1.0 °/t Show Material materials with Biegewinkel 90° of 1.0 °/t | O | EN 573-3, EN 485 | ||||
1.5 °/t Show Material materials with Biegewinkel 90° of 1.5 °/t | O | EN 573-3, EN 485 | ||||
2.0 °/t Show Material materials with Biegewinkel 90° of 2.0 °/t | O | EN 573-3, EN 1386 | ||||
2.5 °/t Show Material materials with Biegewinkel 90° of 2.5 °/t | O | EN 573-3, EN 485 | ||||
Dehnung | 6.0 % Show Material materials with Dehnung of 6.0 % | O | EN 573-3, EN 1386 | A50 | ||
8.0 % Show Material materials with Dehnung of 8.0 % | O | EN 573-3, EN 1386 | A50 | |||
10.0 % Show Material materials with Dehnung of 10.0 % | O | EN 573-3, EN 1386 | A50 | |||
12.0 % Show Material materials with Dehnung of 12.0 % | O | EN 573-3, EN 1386 | A100 | |||
12.0 % Show Material materials with Dehnung of 12.0 % | O | EN 573-3, EN 1386, EN 755 | A50 | |||
13.0 % Show Material materials with Dehnung of 13.0 % | O | EN 573-3, EN 754 | A50 | |||
14.0 % Show Material materials with Dehnung of 14.0 % | O | EN 573-3, EN 755 | A100 | |||
14.0 % Show Material materials with Dehnung of 14.0 % | O | EN 573-3, EN 485 | A50 | |||
15.0 % Show Material materials with Dehnung of 15.0 % | O | EN 573-3, EN 754 | A100 | |||
16.0 % Show Material materials with Dehnung of 16.0 % | O | EN 573-3, EN 485 | A100 | |||
16.0 % Show Material materials with Dehnung of 16.0 % | O | EN 573-3, EN 485 | A50 | |||
17.0 % Show Material materials with Dehnung of 17.0 % | O | EN 573-3, EN 485 | A50 | |||
18.0 % Show Material materials with Dehnung of 18.0 % | O | EN 573-3, EN 485 | A50 | |||
20.0 °C | 9.0 % Show Material materials with Dehnung of 9.0 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Wire | A100 | |
20.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Wire | A10 | |
20.0 °C | 15.0 % Show Material materials with Dehnung of 15.0 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Sheet, Strip | A10 | |
20.0 °C | 18.0 % Show Material materials with Dehnung of 18.0 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Sheet, Strip | ||
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | |||
20.0 °C | 68.0 - 73.0 GPa Show Material materials with Elastizitätsmodul of 68.0 - 73.0 GPa | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Sheet, Strip, Wire | ||
Härte, Brinell | 40.0 [-] Show Material materials with Härte, Brinell of 40.0 [-] | O | EN 573-3, EN 485 | |||
20.0 °C | 35.0 [-] Show Material materials with Härte, Brinell of 35.0 [-] | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Sheet, Strip, Wire | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Schubmodule | 26.4 GPa Show Material materials with Schubmodule of 26.4 GPa | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | |||
20.0 °C | 26.0 - 27.0 GPa Show Material materials with Schubmodule of 26.0 - 27.0 GPa | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Sheet, Strip, Wire | ||
Zugfestigkeit | 150.0 MPa Show Material materials with Zugfestigkeit of 150.0 MPa | O | EN 573-3, EN 1386, EN 485 | |||
155.0 MPa Show Material materials with Zugfestigkeit of 155.0 MPa | O | EN 573-3, EN 485 | ||||
160.0 MPa Show Material materials with Zugfestigkeit of 160.0 MPa | O | EN 573-3, EN 754, EN 755 | ||||
20.0 °C | 110.0 MPa Show Material materials with Zugfestigkeit of 110.0 MPa | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Wire | ||
20.0 °C | 150.0 MPa Show Material materials with Zugfestigkeit of 150.0 MPa | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Sheet, Strip |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.3399999999999996e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3399999999999996e-05 1/K | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3399999999999996e-05 1/K | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | ||
Schmelzpunkt | 585.0 - 650.0 °C Show Material materials with Schmelzpunkt of 585.0 - 650.0 °C | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | ||
Spezifische Wärmekapazität | 896.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 896.0 J/(kg·K) | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | ||
Wärmeleitfähigkeit | 20.0 °C | 170.0 - 220.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 170.0 - 220.0 W/(m·K) | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 24000000.0 - 32000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 24000000.0 - 32000000.0 S/m | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
spezifischer Widerstand | 3.13e-08 - 4.17e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.13e-08 - 4.17e-08 Ω·m | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493 | Sheet, Strip, Wire |
0.50 % Show Material materials with Eisen of 0.50 % | O | EN 573-3, EN 1386, EN 485, EN 754, EN 755 | ||
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
Magnesium | 0.6 - 1.2 % Show Material materials with Magnesium of 0.6 - 1.2 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
Mangan | 0.4 - 1.0 % Show Material materials with Mangan of 0.4 - 1.0 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
Silizium | 0.7 - 1.3 % Show Material materials with Silizium of 0.7 - 1.3 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | O | DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 240, VdTÜV WB 414, VdTÜV WB 327, VdTÜV WB 423, VdTÜV WB 493, EN 1386, EN 485, EN 754, EN 755 | Sheet, Strip, Wire |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: acceptable, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): good / sufficient, friction soldering: good, soft brazing with flux: acceptable | |
Corrosion properties | Seawater: good, weathering: very good | |
Workability | Bending / Spinning (cold): acceptable (T3, T4) / good (O), Impact extrusion (cold): good (O), Deep drawing / upsetting (Condition) good (O) / good (O) |