DIN 1725-1 Grade 3.4345 T6

View suppliers (3)
Want to keep this datasheet? Save it now in your required format

Description

The alloy AlZnMgCu0,5 belongs to the aluminum materials, which achieve very high mechanical strength. With hot ageing the strength grade F 49 is attainable. This alloy is good splinter-giving machinably. The alloy is weldable with consideration of certain conditions, especially a heat influence zone with small strength appears there. One should not weld therefore if possible. A good corrosion resistance can be only guaranteed, if an appropriate protective surface layer is present. The corrosion resistance improves noticeably also by hot ageing. Roll-plating of sheet metals of this alloy e.g. with AlZn1 will support the small corrosion resistance with exhaust the high mechanical strenght fully. Thus the area of application extends noticeably. This alloy possesses well splinter-giving workability. Heat treatment for hardening: solution annealing: 470 to 480 °C, quenching in water hot ageing: 12 to 24 h at 115 to 125 °C, 4 to 6 h at 165 to 180 °C (two stage ageing) cold ageing is uncommon Application: In mechanical engineering for devices, tools. Predominantly tension-poor strained sheet metals for baseplates, head and stamp retaining plates as well as in the automobile engineering for safety-related parts and bumpers.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM,AluKey zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueConditionRelated StandardsShape

Dichte

2.78 g/cm³

Show Material materials with Dichte of 2.78 g/cm³

T6

EN 573-3, EN 485, EN 754, EN 755

20.0 °C

2.78 g/cm³

Show Material materials with Dichte of 2.78 g/cm³

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

Mechanisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Dehnung

3.0 %

Show Material materials with Dehnung of 3.0 %

T6

EN 573-3, EN 485

A100

5.0 %

Show Material materials with Dehnung of 5.0 %

T6

EN 573-3, EN 485

A100

5.0 %

Show Material materials with Dehnung of 5.0 %

T6

EN 573-3, EN 755

A50

6.0 %

Show Material materials with Dehnung of 6.0 %

T6

EN 573-3, EN 754

A50

7.0 %

Show Material materials with Dehnung of 7.0 %

T6

EN 573-3, EN 485, EN 755

A100

8.0 %

Show Material materials with Dehnung of 8.0 %

T6

EN 573-3, EN 485, EN 754

A100

8.0 %

Show Material materials with Dehnung of 8.0 %

T6

EN 573-3, EN 485, EN 754

A50

20.0 °C

2.0 %

Show Material materials with Dehnung of 2.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

20.0 °C

3.0 %

Show Material materials with Dehnung of 3.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

20.0 °C

4.0 %

Show Material materials with Dehnung of 4.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

20.0 °C

6.0 %

Show Material materials with Dehnung of 6.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

Elastizitätsmodul

70.0 GPa

Show Material materials with Elastizitätsmodul of 70.0 GPa

T6

EN 573-3, EN 485, EN 754, EN 755

20.0 °C

72.0 GPa

Show Material materials with Elastizitätsmodul of 72.0 GPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

Härte, Brinell

121.0 [-]

Show Material materials with Härte, Brinell of 121.0 [-]

T6

EN 573-3, EN 485

127.0 [-]

Show Material materials with Härte, Brinell of 127.0 [-]

T6

EN 573-3, EN 485

133.0 [-]

Show Material materials with Härte, Brinell of 133.0 [-]

T6

EN 573-3, EN 485

20.0 °C

130.0 [-]

Show Material materials with Härte, Brinell of 130.0 [-]

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

20.0 °C

135.0 [-]

Show Material materials with Härte, Brinell of 135.0 [-]

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 7000 Series Aluminium

Poissonzahl

0.33 [-]

Show Material materials with Poissonzahl of 0.33 [-]

Typical for Wrought 7000 Series Aluminium

Schubmodule

20.0 °C

27.5 GPa

Show Material materials with Schubmodule of 27.5 GPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

Zugfestigkeit

410.0 MPa

Show Material materials with Zugfestigkeit of 410.0 MPa

T6

EN 573-3, EN 485

430.0 MPa

Show Material materials with Zugfestigkeit of 430.0 MPa

T6

EN 573-3, EN 485

450.0 MPa

Show Material materials with Zugfestigkeit of 450.0 MPa

T6

EN 573-3, EN 485

460.0 MPa

Show Material materials with Zugfestigkeit of 460.0 MPa

T6

EN 573-3, EN 754

470.0 MPa

Show Material materials with Zugfestigkeit of 470.0 MPa

T6

EN 573-3, EN 755

490.0 MPa

Show Material materials with Zugfestigkeit of 490.0 MPa

T6

EN 573-3, EN 755

20.0 °C

440.0 MPa

Show Material materials with Zugfestigkeit of 440.0 MPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

20.0 °C

450.0 MPa

Show Material materials with Zugfestigkeit of 450.0 MPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

20.0 °C

460.0 MPa

Show Material materials with Zugfestigkeit of 460.0 MPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

20.0 °C

470.0 MPa

Show Material materials with Zugfestigkeit of 470.0 MPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

20.0 °C

480.0 MPa

Show Material materials with Zugfestigkeit of 480.0 MPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

Thermisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Koeffizient der thermischen Ausdehnung

20 °C

2.36e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K

T6

EN 573-3, EN 485, EN 754, EN 755

100 °C

2.36e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K

T6

EN 573-3, EN 485, EN 754, EN 755

Schmelzpunkt

480.0 - 640.0 °C

Show Material materials with Schmelzpunkt of 480.0 - 640.0 °C

T6

EN 573-3, EN 485, EN 754, EN 755

Spezifische Wärmekapazität

795.0 - 1050.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 795.0 - 1050.0 J/(kg·K)

Typical for Wrought 7000 Series Aluminium

Wärmeleitfähigkeit

20.0 °C

130.0 - 160.0 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 130.0 - 160.0 W/(m·K)

T6

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Forging

Elektrisch

PropertyTemperatureValueConditionRelated StandardsShape

Elektrische Leitfähigkeit

20.0 °C

19000000.0 - 23000000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 19000000.0 - 23000000.0 S/m

T6

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Forging

spezifischer Widerstand

4.35e-08 - 5.26e-08 Ω·m

Show Material materials with spezifischer Widerstand of 4.35e-08 - 5.26e-08 Ω·m

T6

EN 573-3, EN 485, EN 754, EN 755

Chemical properties

PropertyValueConditionRelated StandardsShape

Chrom

0.1 - 0.3 %

Show Material materials with Chrom of 0.1 - 0.3 %

T6

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Forging

Eisen

0.5 %

Show Material materials with Eisen of 0.5 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Forging

0.50 %

Show Material materials with Eisen of 0.50 %

T6

EN 573-3, EN 485, EN 754, EN 755

Kupfer

0.5 - 1.0 %

Show Material materials with Kupfer of 0.5 - 1.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Forging

Magnesium

2.6 - 3.7 %

Show Material materials with Magnesium of 2.6 - 3.7 %

T6

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Forging

Mangan

0.1 - 0.4 %

Show Material materials with Mangan of 0.1 - 0.4 %

T6

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Forging

Silizium

0.5 %

Show Material materials with Silizium of 0.5 %

T6

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Forging

Zink

4.3 - 5.2 %

Show Material materials with Zink of 4.3 - 5.2 %

T6

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 754, EN 755

Forging

Technological properties

Property
Anodizing

decorative: not suitable, Protective: good

Brazing

hard brazing (with flux/ without flux): not suitable / not suitable, friction soldering: not suitable, soft brazing with flux: not suitable

Corrosion properties

Seawater: poor, weathering: sufficient

Workability

Bending / Spinning (cold): poor (O) / not suitable, Impact extrusion (cold): not suitable, Deep drawing / upsetting (Condition) not suitable / not suitable