Chemical properties
Property | Value |
---|---|
Aluminium | 9.6 - 11 % Show Material materials with Aluminium of 9.6 - 11 % |
Andere | Rest Cu, total 2.8 |
Antimon | 0.05 % Show Material materials with Antimon of 0.05 % |
Arsen | 0.05 % Show Material materials with Arsen of 0.05 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Mangan | 1.5 - 2.3 % Show Material materials with Mangan of 1.5 - 2.3 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Phosphor | 0.1 % Show Material materials with Phosphor of 0.1 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 1.5 % Show Material materials with Zink of 1.5 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |