Aluminium: 9.6 - 11 %

Quick Comparison

Wrought Copper Bronze Aluminium Bronze

AMPCO® 45 Extruded and drawn rods

Geliefert von:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

Aluminum Nickel Bronze TQ50 Tube (C95510)

Geliefert von:

Materion Brush GmbH

Cast Copper Bronze Aluminium Bronze

Aluminum Nickel Bronze TQ50 Tube (C95520)

Geliefert von:

Materion Brush GmbH

Cast Copper Bronze Aluminium Bronze

AMPCO® M4 Centrifugal castings

Geliefert von:

AMPCO METAL

Wrought Copper Bronze Aluminium Bronze

AMPCO® M4 Extrusions

Geliefert von:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® M4 Sand castings

Geliefert von:

AMPCO METAL

Nickel Chromium Iron Alloy

Sanicro® 69

Geliefert von:

Alleima (formerly Sandvik Materials Technology)

Cast Copper Bronze Aluminium Bronze

AMPCO® 18.23 Centrifugal castings

Geliefert von:

AMPCO METAL

Wrought Copper Bronze Aluminium Bronze

AMPCO® 18 Extruded and drawn rounds and rectangular bars

Geliefert von:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® 18.23 Continuous cast

Geliefert von:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® 18.23 Sand castings

Geliefert von:

AMPCO METAL

Wrought Copper Bronze Aluminium Bronze

UNS C63000 / AMS 4640 Bronze

Cast Copper Bronze Aluminium Bronze

AMPCO® 18 Centrifugal castings

Geliefert von:

AMPCO METAL

Wrought Copper Bronze Aluminium Bronze

AMPCO® 18 Forgings

Geliefert von:

AMPCO METAL

Wrought Copper Bronze Aluminium Bronze

AMPCO® 18 Rolled

Geliefert von:

AMPCO METAL
Seite 1 von 19