Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 5 % Show Material materials with Dehnung of 5 % | |
Elastizitätsmodul | 23.0 °C | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze |
Härte, Brinell | 23.0 °C | 170 - 185 [-] Show Material materials with Härte, Brinell of 170 - 185 [-] | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze |
Streckgrenze Rp 0,2 | 23.0 °C | 320 - 380 MPa Show Material materials with Streckgrenze Rp 0,2 of 320 - 380 MPa | |
Zugfestigkeit | 23.0 °C | 680 - 750 MPa Show Material materials with Zugfestigkeit of 680 - 750 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze | |
Spezifische Wärmekapazität | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 10 - 12 % Show Material materials with Aluminium of 10 - 12 % |
Andere | for Mould cast (Ingot metals and Castings): Fe > 3.0. Al > 9.0. Cu < 84.5 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 4 - 7 % Show Material materials with Eisen of 4 - 7 % |
Kupfer | 72 - 78 % Show Material materials with Kupfer of 72 - 78 % |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % |
Mangan | 2.5 % Show Material materials with Mangan of 2.5 % |
Nickel | 4 - 7.5 % Show Material materials with Nickel of 4 - 7.5 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |