Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN CB483K

Ingot

EN CB483K, EN CuSn12-B

EN CB491K

Ingot

EN CB491K, EN CuSn5Zn5Pb5-B

EN CB752S

Ingot

EN CB752S, EN CuZn35Pb2Al-B

EN CB753S

Ingot

EN CB753S, EN CuZn37Pb2Ni1AlFe-B

EN CB754S

Ingot

EN CB754S, EN CuZn39Pb1Al-B

EN CB755S

Ingot

EN CB755S, EN CuZn39Pb1Al-B

EN CC331G

Bar

EN CC331G, EN CuAl10Fe2-C

EN CC333G

Bar

EN CC333G, EN CuAl10Fe5Ni5-C

EN CC334G

Bar

EN CC334G, EN CuAl11Fe6Ni6-C

EN CC481K

Bar

EN CC481K, EN CuSn11P-C

Showing 1 to 10 of 86 entries

Previous

1
2
3
...
9

Next

Locations

Israel

Israel

Hazait St. Alon Tavor industrial zone, P.O. Box 1202

1811102 Afula

(+972)48477500

United States

United States

2638 United Lane

60007 Elk Grove Village,Illinois

(+1)8472327115