Chemical properties
Property | Value |
---|---|
Aluminium | 1E-3 % Show Material materials with Aluminium of 1E-3 % |
Andere | Rest Zn, total 0.2. excluded Fe |
Antimon | 0.01 % Show Material materials with Antimon of 0.01 % |
Arsen | 1E-3 % Show Material materials with Arsen of 1E-3 % |
Bismut | 0.01 % Show Material materials with Bismut of 0.01 % |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Cadmium | 0.03 % Show Material materials with Cadmium of 0.03 % |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % |
Kupfer | 58.5 - 61.5 % Show Material materials with Kupfer of 58.5 - 61.5 % |
Mangan | 0.05 - 0.25 % Show Material materials with Mangan of 0.05 - 0.25 % |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |