Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 7 % Show Material materials with Dehnung of 7 % | |
Elastizitätsmodul | 23.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Elongation A100 | 23.0 °C | 3 % Show Material materials with Elongation A100 of 3 % | |
Härte, Brinell | 23.0 °C | 90 [-] Show Material materials with Härte, Brinell of 90 [-] | |
Härte, Vickers | 23.0 °C | 90 [-] Show Material materials with Härte, Vickers of 90 [-] | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Streckgrenze Rp 0,2 | 23.0 °C | 200 MPa Show Material materials with Streckgrenze Rp 0,2 of 200 MPa | |
Zugfestigkeit | 23.0 °C | 250 MPa Show Material materials with Zugfestigkeit of 250 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | |
100.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | ||
Schmelzpunkt | 965 - 1100 °C Show Material materials with Schmelzpunkt of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper | |
Spezifische Wärmekapazität | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Wärmeleitfähigkeit | 23.0 °C | 368 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 368 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.45E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 5.45E+7 S/m |
spezifischer Widerstand | 23.0 °C | 1.83E-8 Ω·m Show Material materials with spezifischer Widerstand of 1.83E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.1 |
Phosphor | 0 - 0.01 % Show Material materials with Phosphor of 0 - 0.01 % |
Tellur | 0.4 - 0.7 % Show Material materials with Tellur of 0.4 - 0.7 % |